APPARATUS FOR STABILITY TO MIXING WITH CEMENT - IS 8887, ANNEX-G
As per IS:8887-2018 (Annex.G)
APPARATUS FOR COATING ABILITY AND WATER RESISTANCE - IS 8887:2018 (ANNEX F)
The test determines the coating ability and water resistance of bitumen emulsions. It assesses the emulsion's capacity to coat aggregate surfaces uniformly and retain the coating after immersion in water, which is crucial for performance in road construction and maintenance. As per IS 8887:2018 (Annex F), AASHTO T59, EN 13808, ASTM D244.
APPARATUS FOR DETERMINATION COAGULATION OF EMULSION - IS-8887, Annex- C
Apparatus for determination of Coagulation of Emulsion at low temperature as per IS-8887 Annex- C, consisting of 2 nos. glass boiling tube (150 X 25mm) with cork with central hole 2 nos. sieve 600 microns, 4 nos. 600ml. beakers and water bath thermostatically controlled for 2 holes.
APPARATUS FOR DETERMINATION OF STORAGE STABILITY - IS 8887, ASTM D6930
The test method for storage stability in IS 8887 involves placing a sample of the bitumen emulsion in a cylindrical container and allowing it to stand undisturbed for a specified period, typically 24 hours. After the settling period, samples are taken from the top and bottom of the container, and the difference in bitumen content between the top and bottom is measured.
MARSHAL STEEL BLOCK-102MM DIA X 50 MM HEIGHT-FOR HEATING THE COMPACTION HAMMER FOOT
For heating the compaction hammer foot. Weight : 03 Kgs. Dimensions : 102 mm dia x 50 mm height
DIGITAL VACUUM REGULATOR FOR KINEMATIC VISCOSITY BATH-FOR 4 VISCOMETERS
For Precise Measurement and Control of Vacuum at 300 mm Hg Below Atmospheric Pressure: Ideal for method ASTM D2171
DIRECT READING DIGITAL PENETROMETER - FOR BITUMEN
As per IS 1203, IS 1448. ASTM D5. In addition to regular features, this model is Fitted with Micrometer differential gearing system for fine movement of penetration needle. Complete with Automatic Digital Timer, Digital Penetration indicator, Penetration cup and transfer dish. Water bath to condition the sample is available at extra cost.
RUBBER CONTENT OF CRUMB RUBBER MODIFIED BITUMEN- SOXHLET METHOD
As per As per ASTM D6814, AASHTO M-320, AUSTROADS TEST METHOD AGPT/T142. To determine the rubber content of crumb rubber modified bitumen (CRMB) using a Soxhlet extraction method. The rubber in crumb rubber modified bitumen is extracted using a suitable solvent in a Soxhlet extractor. The non-rubber component (bitumen) dissolves in the solvent, leaving the rubber residue, which is then weighed to determine the rubber content.
APPARATUS FOR DETERMINATION OF WAX CONTENT WITH ACCESORIES AS PER IS 10512-2003
This instrument is used for the determination of the paraffin wax content of bitumen and bituminous binder by distillation.